Large Pores Dominate Flow Through Nanomembranes (FOW)

Because of the non-linear dependence of volumetric flow rate on pore size … where t is the membrane thickness and r is the pore radius, large pores contribute disproportionately to the total flow through a membrane than small pores. The

NPN Clogging with Particle Size and Concentration (FOW)

This figure appears in our 2016 JMS paper and describes the clogging behavior of NPN with a 37 nm average pore size. The y-axis is the volume of filtrate after 1 min of forward centrifugation at 690g (3000 RPM). The