Table of Gas Permeance and Water Permeabilities for Various Nanomembranes

Wright, E., Miller, J.J, Csorda, M.. Gosselin, A.R., Carter, J.A., McGrath, J.L., Latulippe, D.R., Roussie, J.A. (2020) Development of Isoporous Microslit Silicon Nitride Membranes for Sterile Filtration Applications Biotechnology & Bioengineering https://doi.org/10.1002/bit.27240

DesOrmeaux, J. P., Winans, J. D., Wayson, S. E., Gaborski, T. R. , Khire, T. S., Striemer, C. C., and McGrath, J. L. (2014) Nanoporous silicon nitride membranes fabricated from porous nanocrystalline silicon templates, Nanoscale 6:10798-10805

About

Professor McGrath holds a BS degree in Mechanical Engineering from Arizona State and a MS degree in Mechanical Engineering from MIT. He earned a PhD in Biological Engineering from Harvard/MIT's Division of Health Sciences and Technology. He then trained as a Distinguished Post-doctoral Fellow in the Department of Biomedical Engineering at the Johns Hopkins University. Professor McGrath has been on the Biomedical Engineering faculty at the University of Rochester since 2001 where he also serves as the director of the graduate program BME and associate director of the URNano microfab and metrology core. McGrath's research was focused on the phenomena of cell migration until 2007 when he founded the interdisciplinary Nanomembrane Research Group to development and apply silicon membrane technologies. Professor McGrath is also a co-founder and past president of SiMPore Inc., a company founded to commercially manufacture silicon membranes and related technologies.

Leave a Reply