Description
Membrane Thickness: 400 nm
Pore Size: 0.5 µm
Porosity: 18% – 22%
Window Pattern / Format: (3 slot): 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
Membrane Thickness: 400 nm
Pore Size: 0.5 µm
Porosity: 18% – 22%
Window Pattern / Format: (3 slot): 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
| Lot Number ( | Mean Pore Size (nm) +/- 1 Std | Morphology |
| 5106B | 543.66 +/- 17.37 | smooth |
| 5107 | 393.98 +/- 20.02 | rough |
| 5104 | 445.51 +/- 16.78 | smooth |
| 5122 | 409.42 +/- 20.88 | rough |
| 5103 | 523.98 +/- 17.96 | rough |
| 5189 | ||
| 5244 | ||
| 5245 | ||
| 5246 |