0.5 μm Microslit

SKU: MSSN400-3L-0.5 Category:

Description

Membrane Thickness: 400 nm

Pore Size: 0.5 µm

Porosity: 9% – 12%

Window Pattern / Format: (3 slot): 0.7 mm x 2 mm

This product comes in quantities as indicated by the individual lot title.

Lot Number Porosity (%) +/- 1 Std Mean Pore Size (nm) +/- 1 Std Morphology
5150 10.1% (SiMPore) 0.47 (SiMPore)