0.5 μm Microporous

SKU: MPSN400-3L-0.5HP Categories: ,

Description

Membrane Thickness: 400 nm

Pore Size: 0.5 µm

Porosity: 18% – 22%

Window Pattern / Format: (3 slot): 0.7 mm x 2 mm

This product comes in quantities as indicated by the individual lot title.

Lot Number ( Mean Pore Size (nm) +/- 1 Std Morphology
5106B 543.66 +/- 17.37 smooth
5107 393.98 +/- 20.02 rough
5104 445.51 +/- 16.78 smooth
5122 409.42 +/- 20.88 rough
5103 523.98 +/- 17.96 rough
5189
5244
5245
5246