Description
Membrane Thickness: 400 nm
Pore Size: 0.5 µm
Porosity: 9% – 12%
Window Pattern / Format: (3 slot): 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
Membrane Thickness: 400 nm
Pore Size: 0.5 µm
Porosity: 9% – 12%
Window Pattern / Format: (3 slot): 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
| Lot Number | Porosity (%) +/- 1 Std | Mean Pore Size (nm) +/- 1 Std | Morphology |
| 5150 | 10.1% (SiMPore) | 0.47 (SiMPore) | |