1 μm Microslit

SKU: MSSN400-3L-1.0 Categories: ,

Description

Membrane Thickness: 400 nm

Pore Size: 1 µm

Porosity: 9% – 12%

Window Pattern / Format: (3 slot): 0.7 mm x 2 mm

This product comes in quantities as indicated by the individual lot title.

Lot Number Porosity (%) +/- 1 Std Mean Pore Size (nm) +/- 1 Std Morphology