3 Slot Nonporous

SKU: SN400-3L Categories: ,

Description

Membrane Thickness: 400 nm

Pore Size: N/A

Porosity: N/A

Window Pattern / Format: 0.7 mm x 2 mm

This product only comes in pairs of 2.

Lot Number Porosity (%) +/- 1 Std Mean Pore Size (nm) +/- 1 Std Morphology
Unknown N/A N/A N/A