Description
Membrane Thickness: 100 nm
Pore Size: 35 – 65 nm + 3 µm
Porosity: NPN cell culture grade plus ~5% for 3 µm micropores
Window Pattern / Format: 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
Membrane Thickness: 100 nm
Pore Size: 35 – 65 nm + 3 µm
Porosity: NPN cell culture grade plus ~5% for 3 µm micropores
Window Pattern / Format: 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
| Lot Number | Mean Pore Size (um) | Pore Density (pores/mm^2) | % Micropore Porosity |