Description
Membrane Thickness: 100 nm
Pore Size: 35 nm – 65 nm
Porosity: ~9% – 18%
Window Pattern / Format: 4 x: 0.3 mm x 3 mm
This product comes in quantities as indicated by the individual lot title.
Membrane Thickness: 100 nm
Pore Size: 35 nm – 65 nm
Porosity: ~9% – 18%
Window Pattern / Format: 4 x: 0.3 mm x 3 mm
This product comes in quantities as indicated by the individual lot title.
| Lot Number | Porosity (%) +/- 1 Std | Mean Pore Size (nm) +/- 1 Std | Morphology |
| 1508 |