Description
Membrane Thickness: 100 nm
Pore Size: 35 – 65 nm + 5 µm
Porosity: NPN cell culture grade plus 0.1% – 2.5% for 5 µm
Window Pattern / Format: 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
Membrane Thickness: 100 nm
Pore Size: 35 – 65 nm + 5 µm
Porosity: NPN cell culture grade plus 0.1% – 2.5% for 5 µm
Window Pattern / Format: 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
| Lot Number | Mean Pore Size (um) | Pore Density (pores/mm^2) | % Micropore Porosity |
| 1495 | |||
| 1496 | 4.77 | 1127 | 2.02% |
| 1479 | 3.07 | 1,026 | 0.76% |