Description
This product can be ordered in quantities of 1 feet. Please review the model numbers below for sizing details.
| Model | 95802-01 |
| Tubing int.Ø | 0.8 mm (0.03125″) |
| Wall Thickness | 0.8 mm (0.03125″) |
| Tubing O.D. | 2.4 mm (0.09375″) |
| Tubing material | Platinum-cured silicone |
| Color | Translucent |
| Length | 7.6 m (25 ft.) |
| Clarity | Translucent |
| GMP compliant | Yes |
| Length per pack | 7.6 m (25 ft.) |
| Max. Pressure | 2.1 bar (30 psi) |
| Max. Temperature | 230 °C (446 °F) |
| Min. Temperature | –50 °C (–58 °F) |
| Regulatory approvals | FDA;USP |
| Sterilisation method autoclave | Yes |
| Sterilisation method EtO | Yes |
| Sterilisation method gamma | Yes |
| Working Pressure | 2.1 bar (30 psi) |
| Model | 95802-00 |
| Tubing int.Ø | 0.5 mm (0.02″) |
| Wall Thickness | 0.8 mm (0.03125″) |
| Tubing O.D. | 2.1 mm (0.0833″) |
| Tubing material | Platinum-cured silicone |
| Color | Translucent |
| Length | 7.6 m (25 ft.) |
| Clarity | Translucent |
| GMP compliant | Yes |
| Length per pack | 7.6 m (25 ft.) |
| Max. Pressure | 2.1 bar (30 psi) |
| Max. Temperature | 230 °C (446 °F) |
| Min. Temperature | –50 °C (–58 °F) |
| Regulatory approvals | FDA;USP |
| Sterilisation method autoclave | Yes |
| Sterilisation method EtO | Yes |
| Sterilisation method gamma | Yes |
| Working Pressure | 2.1 bar (30 psi) |