Description
Membrane Thickness: 100 nm
Pore Size: 35 nm – 65 nm
Porosity: ~9% – 27%
Window Pattern / Format: 0.7 mm x 2 mm
Membrane Thickness: 100 nm
Pore Size: 35 nm – 65 nm
Porosity: ~9% – 27%
Window Pattern / Format: 0.7 mm x 2 mm
| Lot Number | Porosity (%) +/- 1 Std | Mean Pore Size (nm) +/- 1 Std | Morphology |
| 1515 | 13.2 ± 0.5 | 46.5 ± 1.3 | Standard |
| 1522 | 13.6 ± 0.9 | 60.1 ± 2.6 | Standard |
| 1512 | 15.0 ± 0.9 | 61.9 ± 1.6 | Standard |
| 1523 | 13.7 ± 0.9 | 54.2 ± 1.5 nm | Standard |
| 1526 | 15.5 (SiMPore) | 49.2 nm (SiMPore) | NA |
| 1540 | 9.9 +/- 0.8% | 42.2 +/- 1.0 nm | Standard |
| 1524 | 15.3 +/- 1.4% | 59.9 +/- 2.8 nm | Standard |
| 1525 | 12.5 +/- 0.95% | 59.5 +/- 1.5 nm | Standard |
| 1548 | 7.5+/- 0.65% | 45.5 +/- 1.6 nm | Standard |
| 1549 | 7.3+/- 0.5% | 53.55 +/- 2.65 nm | Standard |
| 1550 | 11.27% (no Std) | 55.7 +/- 17.9 nm | Standard |
| 1551 | 8.78% (no Std) | 50.01 +/- 15.58 nm | Standard |
| 1552 | 12.89% | 60.9 +/- 14.92 nm | Standard |
| 1553 | 11.95% | 65.93 +/- 16.64 nm | Standard |
| 240803-20 | 10.1% | 51.81 +/- 13.49 nm | Standard |
| 240803-3 | 13.83% | 55.6 +/- 14.8 | Standard |
| 240803-4 | 15.32% | 58.38 +/- 15.11 nm | Standard |
| 240803-12 | 9.99% | 50.62 +/- 14.61 nm | Standard |
| 240803-13 | 13.45% | 50.66 +/- 14.14% | Standard |
| 240919-17 | 8.19% | 55.33 +/- 14.11 nm | Standard |
| 240919-25 | 11.11% | 61.58 +/- 15.52 nm | Standard |
| 240919-18 | 9.56% | 54.54 +/- 14.53 nm | Standard |
| 240919-14 | 12.45% | 57.92 +/- 16.09 nm | Standard |
| 240917-01 | 9.11% | 53.65 +/- 19.2 nm | Standard |
| 240803-20 | 10.1% | 51.81 +/- 13.49 nm | Standard |
| 240919-13 | 12.09% | 55.25 +/- 13.24 nm | Standard |
| 240919-16 | 4.27% | 50.13 +/- 11.42 nm | Underdeveloped |
| 240803-19 | 11.52% | 54.25 +/- 15.63 nm | Standard |
| 240803-14 | 15.49% | 64.4 +/- 14.62 nm | Standard |