Description
Membrane Thickness: 100 nm
Pore Size: 35 nm – 65 nm
Porosity: ~9% – 18%
Window Pattern / Format: 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
Membrane Thickness: 100 nm
Pore Size: 35 nm – 65 nm
Porosity: ~9% – 18%
Window Pattern / Format: 0.7 mm x 2 mm
This product comes in quantities as indicated by the individual lot title.
| Lot Number | Porosity (%) +/- 1 Std | Mean Pore Size (nm) +/- 1 Std | Morphology |
| 1481 | 16.4 ± 0.4 | 61.2 ± 0.9 | Standard |
| 1519 | 14.2 ± 0.5 | 58.4 ± 1.7 | Standard |
| 1537 | 8.8 ± 08 | 49.1 ± 2.4 | Underetched |
| 1532 | 10.9 ± 1.8 | 54.0 ± 4.3 | Standard |
| 1534 | 11.93% | 47.58 +/- 12.64 nm | Standard |
| 240803-06 | 14.35% | 50.85 +/- 13.42 nm | Standard |
| 240803-07 | 14.87 % | 57.09 +/- 15.05 | Standard |
| 240803-08 | 12.24% | 56.73 +/- 16.12 nm | Standard |
| 240803-09 | 11.72% | 52.42 +/- 15.33 nm | Standard |
| 240803-10 | 14.76% | 55.13 +/- 14.79 nm | Standard |
| 240803-11 | 14.06% | 51.54 +/- 13.98 nm | Standard |