Ultrathin Freestanding Nafion Membrane

Utilizing a cation-exchange membrane like Nafion makes it possible to electrically induce the concentration difference across the membrane. The resulting osmosis of water augments the overall flowrate in addition to the electroosmosis. The thinner the membrane, the stronger the osmotic…

Posted in NRG

Using osmotic pressure to suppress back pressure

The basic principle of inducing the osmotic pressure to suppress back pressure is based on the counterbalance of the opposing flows of solvent.  Consider an electrolytic cell composed of a pair of Ag/AgCl electrodes and a Nafion-coated pnc-Si membrane separating…

Posted in NRG

Promoting adhesion of Nafion on silica using aminosilane

Aminosilane has been used widely to derivatize the surface of silica for the applications in analytical chemistry, biochemistry, and biomedicine. It also plays an important role in providing adhesion for Nafion coating on silica surface. The basic principle is described…

Posted in NRG

EO at 1 mM vs 100 mM salts & the role of a meniscus in pressure measurements

Presentation from yesterday: PPT, PDF

Posted in NRG