Author: Josh Winans
Josh is a postdoc in the McGrath lab working on disruptive membrane technologies.

Forward vs Reverse Centrifugation (continued again)

As discussed in a previous post, we decided to test chips from wafer #1070 because they have smaller pores than those used in the most recent forward vs. reverse study. In the forward direction, 31 uL of filtrate was passed…

Posted in NRG

High Speed camera recording of NPN membranes bursting

Scott Russell from Mech. E. and Steve Gillmer came over to help Sarah and I try to record the burst of membranes at up to 2000 frames per second.  Generally we used 100o frames per second because it was the…

Posted in NRG

Aggregation of 20 nm NPs, IgG, and Tween 20

We had previously tested different surfactants to see if we could get 20 nm polystyrene beads and IgG to stay in suspension while filtering with the centrifuge.  We found 0.1% Tween 20 to be sufficient when dealing with 10:1 (5×10^14)…

Posted in NRG

Forward vs Reverse separations (continued)

We have previously tested the effects on filtrate volume after a given time as a function of concentration. Moving forward we want to quantify the improvement in filtrate volume when using reverse centrifugation instead of forward centrifugation. Initially, we attempted…

Posted in NRG

NPN and pnc-Si deflection tests

I went over to RIT to work with JP on measuring the deflection of NPN and pnc-Si membranes as a function of pressure.  JP and Dave Fang did this work years ago, and we want to pick it up again…

Posted in NRG

Separations with NPN at varied concentrations

We are carrying out filtrations using wafer 1085.  We are testing the total volume of filtrate that passes in a given time.  We expect the total filtrate volume to decrease as concentration increases due to more immediate clogging.  Ultimately, we…

Posted in NRG

SEM of Nanoparticles and NPN

Below are various SEMs of  NPN membranes.  (All samples were coated with metal by using the Denton Ag sputterer for 120 s)  These were used samples that have been sitting out in the lab for weeks.  I don’t remember the exact…

Posted in NRG

Permeance tests with new Omega rotameter

Yaron has acquired an Omega rotameter (FL-3803ST) with interchangeable flow tubes.  The tubes operate in three different ranges low (6-61 mL/min, 042-15-N), medium (150-1,682 mL/min, 082-03-N), and High (1,000-23,752 mL/min, 034-39-N).  I’ve attached an excel file with the calibration data…

Posted in NRG, Protocols

NP + IgG cleanup in 0.1% Tween 20

Our previous work with reverse centrifugation NPN membranes has shown that they may work for cleaning up excess protein from conjugated NPs.  This initial success used ~20 nm red fluospheres with membranes from wafer 1070 (10-15%, ~45nm) and unlabeled IgG…

Posted in NRG

Surfactants tested to reduce agglomeration between IgG and 20 nm fluospheres

Mary Lee and I performed a quick test to determine the efficacy of different surfactants at reducing agglomeration between IgG and 20 nm fluospheres. Each solution is a combination of 50 uL 10 mg/mL IgG (in PBS) + 50 uL…