Membrane fabrication – Nanosphere litho

This post is a recap on the nanosphere lithography based membrane patterning process. The results shown here are from a non-optimized run of the process. The image below shows an overview of the fabrication process used.   Below you can…

Posted in NRG

2017 Spring Meeting – Materials Research Society

Hello everyone, this post is a summary/recap of the MRS Spring meeting that was held in Phoenix, Arizona this past week (April 17 – 21). Here is an overview of two sessions: Molecular and colloidal plasmonics – Synthesis and applications…

Posted in NRG

Nanosphere litho quick update

I will keep this post short and start by saying that the process of establishing a reliable set-up for nanosphere deposition, by evaluating the repeatability of the deposition parameters, has been longer than anticipated. The nanospheres self-assemble at the hexane-water…

Posted in NRG

Review paper: Fabrication Techniques Enabling Ultrathin Nanostructured Membranes for Separations

As you may already know, we are writing a review article for the Electrophoresis journal on nanofabrication methods. This post is to request your feedback on the figures included in the manuscript. The main objective of figure 1 is to…

Posted in NRG

Sacrificial releasing layer and SU-8, plans

This post summarizes a quick update on 2 different goals: 1) membrane releasing and 2) SU-8 strain reduction. Here you will find basic background on some of the work that has already been conducted and the planned experimental work that…

Posted in NRG

Review of nano-fabrication

Hello everyone, for my first ever post I would like to share with you a collection of ideas that has turned into a review I’ll be working on. Here you will find some selected publications that report interesting fabrication processes…

Posted in NRG