Cell Proliferation on Different Membrane Porosities and Pore Sizes

To determine whether cell proliferation is a function of membrane porosity and/or pore size, human umbilical vein endothelial cells (HUVECs) were cultured on various surfaces.  The cells were seeded on low and high porosity membranes of 0.5 um and 3.0…

Posted in NRG

Testing CMFDA for Measuring Proliferation

The goal of the experiment was to use a fluorescent dye to label live cells in order to measure proliferation over several days.  To avoid cell toxicity, the intensity of the fluorescence was reduced to ~1.5%.  Human umbilical vein endothelial…

Posted in NRG