Rotation Project Complete: Dialysis of cytochrome c across a commercial membrane

Dan Steiner Rotation Summary Abstract The purpose of this rotation project was to develop and test a clampable system for eventual use in scalable nanomembrane dialysis systems. The nanomembrane dialysis system will be miniaturized into a compact, wearable hemodialysis device that…

Posted in NRG, Protocols

Benchtop dialysis schematic and associated information

Hello All, My name is Dan Steiner and I am a rotation student that has been working with Dean on designing a modular benchtop apparatus to study in vivo blood dialysis. The purpose of this project is to create a…