Author: Jessica Snyder

Gold does not diffuse in DIH20

I set up diffusion experiments using the wafers that Tom was able to pass gold through in DI H2O using pressure.  5nm particles do not pass in 24 or 48 hours.  If we have extra samples I will be testing…

Posted in NRG

TEM Particle Update

This is a reprisal of the old post. While manufacturer declares particles to be 5, 10, etc, they do however give a measured average to their particles in the written material they provide.  I did not have that in the…

Posted in NRG

Reimaging Protein Separations

Originally, I created the following figure to visualize the relationship between sieving coefficient and molecular weight: (originally from this post) I can now take the protein dimensions that I obtained from crystal structures (posted here) and replot this figure: In…

Posted in NRG

Zeta Potentials

This post shows that C-dots are pretty close to neutral.  Here I’ve looked at gold nanoparticles and albumin. 5nm Gold: The distribution is very spread out, but everything centers around -58 mV. 10nm Gold: This sample looks a little bimodal. …

Posted in NRG

Protein Ladder

I’ve tried to collect some information on the protein ladder that we’ve been using for separations.  Sizes have thus far been taken from crystal structures and loosely measured used JMol on the PDB site.  This is meant to just give…

Posted in NRG

Cellulose C-Dot separations

I used 100kD Millipore Celllulose membranes to separate the 2 C-dot particles.  The results are similar to those I’ve obtained with pnc-Si; the 10nm particles pass while the 30nm ones do not. Cy5 10nm particles: Sulforhodamine 30nm particles: Here are…

Posted in NRG

Polymeric Separations

This post outlines two sets of polymer membrane separations using 100kD PES and 30kD cellulose in diffusion mode.  The 100kD PES experiment is a repeat of the experiment found here; in the first trial of this work, there was no…

Posted in NRG

C-dot separations

I performed separations using C-dots from Hybrid Silica, a silica based particle with an internal fluorescent core.  The particles are coated with a PEG layer of unknown length, but the idea would be that they’d be less affected by electrostatics…

Posted in NRG

EO rate changing over time

I have observed that in some cases the rate of EO can go up or down over the course of an experiment.  Often the initial burst in the first 5 minutes is high, then the rate may stabilize or drop. …

Posted in NRG

EO: Carbonized Membranes, Heating

This is a short review of a few experiments that Tom had set up this morning. Carbonized membranes: A few carbonized membranes that were used for permeability measurements were tested in EO.  The membranes were left in the sepcon, which…

Posted in NRG