Author: Kate Busse

PEG Mono-layer Detection on Crosslinked Oxide Chips

Below are the results of my recent crosslinking efforts. PEG with 1.5% crosslinker was exposed to UV light at varying times through a bar  printer/transparency mask measuring 100/200. In theory this corresponds to 100 micron PEG bars and 200 micron…

Posted in NRG

PEG microarray on oxide membrane

We have had success cross-linking PEG to TEOS membranes pretreated with TPM to aid in adhesion. This was done first on nonporous membranes, and then porous. We used 50% PEG at 1.5% cross-linker, which cross-linked at 8000ms. For comparison, 100%…

Posted in NRG

PEG Microarray Solution Dilution and X-linker Concentration Study

Working on the development of PEG microarrays for cell heterogeneity applications. Current work has been accomplished on TPM coated glass coverslips. Transfer to membranes are in progress. Three different x-linker concentrations were tested in a 1:1 mixture of PEG and…

Posted in NRG

Microarray progress: slightly successful seeding and dilution/concentration variations

A control was done to observe cell proliferation on a TPM coated cover glass. Images were taken at 10x after 4 days.  TPM coated cover glass  Polystyrene petri dish We are having some success with the seeding of bend.3 cells…

Posted in NRG

PEG Microarray Developments

Updates: We can now put the glass on top of the mask, which allows the use of nonstick agents in the creation of PEG microarrays. The ability to cross-link PEG-Diacrylate (PEG-DA) with a photoinitator and UV exposure was previously tested and…