Author: Kelly McNabb

SU-8 Surface Modification

Last summer, I attempted to modify the surface of SU-8. The purpose of the experiment was to covalently bond poly(ethylene glycol) (PEG)  to SU-8, which would be useful when the SU-8 is used as a scaffold on the membranes. The…

Posted in NRG

Native Oxide Etching for Micropores SiO2 Membranes

Bob and I are trying to determine which wet etch would be appropriate to use to remove the native oxide inside the pores before membrane liftoff. The issue is when removing the native oxide, we will remove part of the…

Posted in NRG

Successful SiO2 Membrane Liftoff

Bob and I have been busy for the last couple of weeks going through the fabrication process with the hopes of SiO2 membrane liftoff. The fabrication process was similar to the silicon nitride membrane liftoff. The process is shown in…

Posted in NRG

SU-8 Shrinkage

Goal: Measure SU-8 shrinkage that have gone through various soft and hard bake conditions To measure the shrinkage, the SU-8 scaffolds needed to be lifted off, but there was some issues. Originally, the SU-8 was spincoated onto an oxide layer,…

Posted in NRG

PEG Structures with Masks from Laser Printer

The overall goal was to see is if it was possible to create a reliable low resolution mask that can be used for crosslinking PEG structures using a laser printer and transparencies sheets. With these masks, I explored to see…

Posted in NRG