Author: Munther Al-Sudais

History repeats itself: There’s something in the water

Dave Fang posted a poster in 2010 about particles found in DI water. I encountered the same issue during the nano-pocket permeability experiment. He said, “I’ve become increasingly suspicious of membrane clogging during the … permeability experiments.” I conducted an…

Posted in NRG

Nano-pocket Membrane Pressure Modeling

Introduction: In the previous post, we demonstrated our capability to fabricate the nano-pocket membrane and effectively capture and release particles of various sizes. In this post, our focus shifts to exploring the membrane capability. We will focus on the membrane…

Posted in NRG

Nano-pocket Membrane Integration in Tangential Flow for Analyte Capture (TFAC) for Precise Size-Based Particle Capture

Introduction: Building upon previous research conducted by the Gaborski and McGrath labs, this poster introduces a novel approach to isolate extracellular vesicles (EVs) based on size. The earlier work involved the development of a tangential flow membrane capture system to…

Posted in NRG

Fabrication the Nano-pocket membrane (update)

The fabrication of nano pocket membrane to capture and release the EV faced challenges during the etching step. There was a suggestion after the last NRG post to use RIE-2000 located in the UR. This post shows the update on…

Posted in NRG

A new idea to fabricate nano pocket membrane

  Starting in July of 2021, we began a new idea fabricating the nano pocket membrane to capture and release the EVs. From then until now we have successfully fabricated nano pocket membranes by using a lithography method. We faced…

Posted in NRG

Nanopockets membranes for EV’s isolation

 Goal: Is to produce a membrane has pockets to capture the extracellular vesicles EV’s. Membrane structure: Figure 1 shows the membrane structure. The membrane will have two pores sides: upper and lower. The pores on top are bigger than the…