Author: Mike H

BSA does not diffuse through SC269

As I mentioned in the meeting this morning the SC267 samples have run out so I have begun testing SC269 for use in my experiments. This post pertains to a BSA diffusion experiment that I set up yesterday and allowed…

Posted in NRG

UV-Ozone treated SC267: DDM passes and BSA held back

Building on my recent posts I ran an experiment with SC267 testing the ability of BSA and DDM to diffuse through UV-Ozone treated (20min at 150C) and untreated samples. I used four samples testing both BSA and DDM in the…

Posted in NRG

Dye Diffuses through UV-Ozone Treated and Untreated SC267 Samples

In my last post I presented the results of an experiment in which it appeared that BSA did not diffuse through a SC267 sample treated in the UV-Ozone system for 20min at 150C. As a control I also ran BSA…

Posted in NRG

Diffusion of BSA through SC267 prevented using UV-Ozone

As mentioned in my previous few posts Justin and I have been working to characterize contact angles resultant from various exposures in the UV-Ozone system. Earlier this week we got our new oxygen tank installed and it appears that after…

Posted in NRG

UV-Ozone Contact Angle Measurements

Last week I made a post showing the diffusion of DDM and BSA through SC267. I an effort to increase the negative charge associated with the membrane material I proposed using UV-Ozone exposure. A while back there was some concern…

Posted in NRG

BSA diffusion across SC267

Last week I made a post showing detection of detergent diffusion across membrane SC267. In the diffusion set up I had placed 6uL of a 50/50 volume ratio solution of 1.0% DDM and 1mg/mL BSA with 60uL of DI-water on…

Posted in NRG

DDM diffusion through SC267

In a previous post I showed that a colorimetric assay using sulfuric acid and phenol can be used to establish a linear relationship between known detergent concentrations and absorbance values. This assay proves helpful in the project related to Mark…

Posted in NRG

DDM Colorimetric Analysis

After talking with Prahnesh, a graduate student in the Dumont Lab I obtained a protocol for a colorimetric assay used to detect the presence of detergents in solution. The assay uses phenol and concentrated sulfuric acid in the following manner:…

Posted in NRG

BSA-DDM Complex Intensity

I took a look back through the Melvern data I collected, particularly focusing on changes in the intensity data in the BSA-DDM solution (the previously posted plots were of number data). When I compared the peak intensities for BSA, DDM,…

Posted in NRG

BSA Size/Zeta-Potential and BSA-DDM Complex Results

Yesterday I used the Melvern to determine particle size and zeta-potential for BSA in DI-water. For the particle sizing I used a concentration of 2mg/mL but I had to increase the concentration to 10mg/mL in order to get an accurate…

Posted in NRG Tagged with: