Author: Rashmi Sriram

BSA adsorption study on NHS-PEG surfaces-II

I  carried out experiments to test the adsorption of 1 mg/ml of BSA on NHS-PEG surfaces.This time the APTES layer was deposited from solution phase on to the silicon surface in contrast to vapor phase (YES) deposition. Again adsorption of BSA…

Posted in NRG

Effect of NHS- PEG8 modified surfaces on the adsorption of proteins (BSA)

The AIM of this experiment was to see the effect of surfaces modified with PEGs (Polyethylene glycol) to protein adsorption. The PEG that I used for the current study is MS-PEG8 (Methyl-PEG8-NHS) which is Amine reactive. Method: For the current…

Posted in NRG

YES System / Silane Vapor Deposition system – Initial Trials

All the data presented below was generated by Alex from Adarza Biosystems, Inc. Introduction: Chemical vapor deposition of 99% APTES (3-Aminopropyltriethoxysilane) on planar silicon chips was accomplished using the new vapor deposition system (YES: Yield Engineering Systems). In addition to…

Posted in NRG
0
    0
    Your Cart
    Your cart is emptyReturn to Shop