Burst Pressure Probability

Prior Post w/original data and images UPDATE: In the couple plots below, the minimum dimension has been changed to aspect ratio (minimum dimension/maximum dimension): For constant perimeter: alpha=1.1930, beta=.2005, gamma= -0.1380 And for constant area: alpha= -0.1624, beta= -0.0060, gamma=0.2922…