Author: Aslan

NanoParticle Tracking Analysis

Hello Everyone, Kilean helped us to set a training session for NanoParticle Tracking Analysis (NTA) in UR Medical Center. For this training session, i had 4 samples including: Beads, Liposomes, Media + 10% serum, and PBS. Here  is a summary…

Posted in NRG

Exosome Scale Experiments

Hello Everyone, I have been working with Track Etched membranes since last year and we always had problems with leaking and also not being able to push the flow through the membrane. At the end of the summer, i decided…

Posted in NRG

Scale Up Experiments

Hello Everyone, So as you probably remember, we were able to show the capturing and releasing successfully.   In addition, we have a Matlab Code now which helps us for intensity change, so as you can see in the next…

Posted in NRG

Exosome Scale Experiments

Hello Everyone, This is another quick update over our experiments. Exosome Scale Experiments:  In all of our experiments, beads are 100nm and pores are 80nm. As you probably remember, in my last post, i talked about hos the membranes are…

Posted in NRG

Update on Track Etched Membranes Experiments

Hello Everyone, As you probably remember, We have been working on optimizing Track Etched membranes devices since last semester, these membranes are 80 nm pore size and our beads are 100 nm in. We have been working on the design to…

Posted in NRG

Acoustic Based Separation of Nanoparticles

Separation of Nanoparticles using surface acoustic radiation force:  Surface acoustic waves (SAW) can be defined as mechanical waves which propagate on the surface of an elastic medium which most of its energy is concentrated in the surface. It’s been used…

Posted in NRG

Summary for Visiting the Urology lab

Hello Everyone, Here is an update of our meeting in Strong Hospital: So They are working in an urology lab, We met Sam who is a technician in Dr. Carla Beckham’s lab, he is responsible for cell culture part of…

Posted in NRG

Final Update over TE membrane

Hello Everyone,   So first of all, a quick reminder of what i have been working on: we were able to show the trapping of the beads by TE membranes, although in final step and after releasing of the beads,…

Posted in NRG

Optimization of our isolation Technique using Track Etched Membranes

Hello Everyone, Following my experiments with Track Etched Membranes: So we came up with this idea to perform SEM imaging. Following are the images that i took for my experiment with 100 nm beads over 100 nm pores after releasing…

Posted in NRG

Optimization of our isolation technique using Beads

Hello Everyone, I have been working on 100 and 50 nm beads since ACNMM conference to optimize our isolation technique for exosomes and verify that our approach works. Technically, based on the discussion that we had before about Peclet Number,…

Posted in NRG
0
    0
    Your Cart