Manufacturer’s Data Delivery Date: 12/20/2023 (picked up and logged by Ahmet Gurcan) Membrane Type: NPN 1 Slot SKU: NPSN100-1L Lot Number: 1522 Quantity Received: 204 Manufacturer Test Report: Avg Porosity: 14.2%, Avg Pore diameter: 51 nm, Avg flux SLPM at…