The insert was designed for a different chip. We ran it on 3-slot chips anyway to see whether the outer windows break — and whether it matters when they do.
The insert was designed for a different chip. We ran it on 3-slot chips anyway to see whether the outer windows break — and whether it matters when they do.
Six hundred flow insert ports, four numbers each, and a shape score. Shape and aperture turn out to be completely uncorrelated — and the analysis now refuses to guess on the ambiguous ones.
Cells were dying and the bonding region looked yellow. We leached six chips in hot nitric acid and ran 60 elements by ICP-MS. Both chip types look clean.
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A1 (0.63% Porosity – Not real porosity) Lot Number: 250413-25 Quantity Received: 220 Manufacturer Test Report: Average Porosity (nanoporosity): 14.46% Average Diameter (microporous): 3 μm Average…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 2 Slot SKU: NPSN100.C-2LZ.4 Lot Number: 250410-22 Quantity Received: 160 Notes: Manufacturer Test Report: Pore Size: 45.8 nm Porosity: 15.2% Flow Data Avg in SLPM 1psi: 0.18 2psi: 0.35 Burst: 3.67…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MPSN 3 micron Microporous SKU: MPSN400.C-3LX.1-3.0L1 Lot Number: 250409-21 Quantity Received: Manufacturer Test Report: Measured Pore Size: N/A Flow Data Avg in SLPM 2psi: 0.00 4psi: 9.33 15psi: 21.42 Burst: 41.91 PSI…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-18 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 44.4 nm Porosity: 13.5% Flow Data Avg in SLPM 1psi: 0.12 2psi: 0.25 Burst: 3.49…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-10 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 42.2 nm Porosity: 18.8% Flow Data Avg in SLPM 1psi: 0.13 2psi: 0.27 Burst: 2.75…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 2 Slot SKU: NPSN100.C-2LZ.4 Lot Number: 250410-12 Quantity Received: 300 Notes: Manufacturer Test Report: Pore Size: 42.4 nm Porosity: 16% Flow Data Avg in SLPM 1psi: 0.22 2psi: 0.44 Burst: 3.58…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 2 Slot SKU: NPSN100.C-2LZ.4 Lot Number: 250410-14 Quantity Received: 350 Notes: Manufacturer Test Report: Pore Size: 45.8 nm Porosity: 21.7% Flow Data Avg in SLPM 1psi: 0.25 2psi: 0.49 Burst: 2.95…