Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A1 (0.63% Porosity – Not real porosity) Lot Number: 250413-25 Quantity Received: 220 Manufacturer Test Report: Average Porosity (nanoporosity): 14.46% Average Diameter (microporous): 3 μm Average…