Author: Barrett Nehilla

HUVEC Mono(?)layer Na-F Permeability

I had some old HUVEC (P8) on pnc-Si transwells and PET Costar transwells that I didn’t know what to do with.  So I tried a permeability study to see if there were any unexpected roadblocks in the protocol. I seeded…

Posted in NRG

Spinning transwells

In my previous transport post here, I showed O-ring placement data which was motivated by my thinking about the unstirred water layer (UWL).  I think it’s helpful to think about the total resistance to transport through transwell membranes as a…

Posted in NRG

Fluorescein transport: O-ring position and wafer variability

After diffusing through a polymeric or pnc-Si membrane in the transwell format, diffusing molecules meet an “unstirrred water layer = UWL” on the bottom of the membrane.  The UWL acts as another resistance to transport into the receiver compartment.  According…

Posted in NRG

Discoloration – LiCl vs. CsCl vs. NaCl

A couple of weeks ago, I posted a discoloration array experiment that showed monotonic discoloration patterns here.  This was a result that we’d been expecting for several months, but we never got it with NaCl and NaHCO3.  Simplifying the solutions…

Posted in NRG

Sodium fluorescein standard and transport

The last few Tecan posts have dealt with adjusting gain values to optimize fluorescent standard curves.  We now have a general protocol here, and a final standard curve for fluorescein.  Here is the background-reduced standard curve for sodium fluorescein (Na-F)…

Posted in NRG

Detection Limit for Sodium Fluorescein

We now have a linear standard curve for sodium fluorescein (Na-F) in clear 24-well plates.  What is the detection limit? The detection limit is defined as the lowest background-corrected concentration that is 3 standard deviations above the noise of the…

Posted in NRG

Getting linear standard fluorescent curves with the Tecan

Now that we have preliminary transport data from the Tecan, we need standard curves in order to get permeability coefficients. This is really tricky because the RFU (relative fluorescent units) are arbitrary and based on the Tecan gain. For example,…

Posted in NRG

Discoloration Array with NaOH

All of this talk about Zeta Potentials, electro-osmosis and electric double layers got me thinking about these phenomenon in relation to discoloration.  We’ve known that salts accelerate discoloration, and we know that bicarbonate solutions accelerate discoloration as well.  I explained…

Posted in NRG

Fluorescein transport through transwells in 24-well plate

This post is a continuation of the experiments posted a couple of days ago. In that post, I concluded that absorbance measurements of molecules transported through transwells were not possible if the transwell insert was kept in the 24-well during…

Posted in NRG

Carbonization – contact angle and discoloration

Last week, Dave carbonized some w501 samples for me so that I could look into discoloration with this new type of silicon stabilization. The carbonization recipe was: – 1 min 50:1 HF strip to form Si:H – Purge RTP with…

Posted in NRG