PDMS-filled wells don't increase sensitivity for HMM detection

This post is related to the HIV drug screening project that Carrie has been working on.  To refresh everyone’s memory, the aim of this project is to use pnc-Si as a filter to separate high molecular mass (HMM) protein-RNA complexes…

Posted in NRG

Blood-brain barrier co-culture (trial 4)

This is simply the latest repeat of a blood-brain barrier co-culture on PET and pnc-Si transwells.  These are P17 bEnd and P24 NG10815, each seeded at 50000 cells/cm2.  As usual, I seeded bEnd on the pnc-Si side, upside down, and…

Posted in NRG

Cell counts on free-standing vs. supported pnc-Si

In most of the images I’ve posted of bEnd3 on pnc-Si, it seemed like there were more cells crowded onto the free-standing pnc-Si compared to supported pnc-Si.  This post shows that this is indeed true. To do cell counts, I…

Posted in NRG

VEGF expression on pnc-Si transwell

All of my recent posts on VEGF, VEGFR2 and NF-H imunofluorescence have included data from cells grown on coverslips only.  This was my first attempt to try to do immunofluorescence staining on intact pnc-Si transwells and then pop the chips…

Posted in NRG

H2O2 also passes 'non-porous' SC348

In order to validate the salt diffusion test I just posted, I’ve been measuring H2O2 diffusion with SC348 and the Amplex Red Assay from Invitrogen.  I first showed that H2O2 (=34 Da) passed SC348 in this experiment.  Here, I just…

Posted in NRG

Salt diffusion through 'non-porous' SC348

About a month ago, I posted some preliminary data that showed NaCl diffusion through SC348.  This was motivated by my observation of vacuole formation on SC348.  Since my hypothesis is that cell culture substrate permeability is the key factor for…

Posted in NRG

Neurofilament H Immunofluorescence

For my BBB project, I’ve wanted to get nice images of glial cells and endothelial cells on opposite sides of pnc-Si membranes to demonstrate 1) optical transparency 2) that both cell types are in focus (and thus right on top…

Posted in NRG

Cells on squares and slits (2)

I few weeks ago, I had a couple wafers made with different size squares and slits.  I posted my first results here and here.  In that experiment, I showed pretty dramatic 2D structures over both supported and free-standing membranes with…

Posted in NRG

VEGF and VEGFR2 immunofluorescence optimization

Vascular endothelial growth factor (VEGF) is one of the important growth factors/signaling factors that affect endothelial cells.  It is involved in angiogenesis, vessel regrowth during wound healing, vessel development and other vascular functions.  Since this is the most commonly studied…

Posted in NRG

Low density bEnd cells have no vacuoles on pnc-Si

In all of my experiments involving vacuoles, I’ve seeded at 50000 cells/cm2 which gets the cells to confluence after ~ 1 day of growth.  I’ve always seen vacuoles with these parameters.  For this experiment, I wanted to see what the…