Author: Kyle Briggs

Early results with monolith devices

I have had a chance to play with some of the chips from Lot 1278, specifically the design with the 2 micron slots. Results are a bit of a mixed bag. Wetting these chips continues to be a challenge. My…

Posted in NRG

Report on Monolith Devices

I’ve now made 18 pores in monolith devices, with only 1 real success, which was the first one that I report on already. All of the rest have failed for various reasons, mainly relating to the silicon nitride membrane in…

Posted in NRG

First experiments with monoliths

I have three monolith experiments to report, one of which was successful. In all three cases, I was able to make a pore, though it took about 5 times longer than it would have for the NPN-tented chips. This is…

Posted in NRG

Folding Suppression Experiments

A quick recap: of the pores using the old NPN batch, 2 of them showed folding suppression. The first one I was able to collect events for 1000 and 2000 bp dsDNA, bnoth of which showed almost no folding, but…

Posted in NRG Tagged with:

Back to NPN nanofilter experiments

Just a quick update on my status: I got the NPN pre-filters from Greg in Montreal and finished testing 15 of them last week, so this week I will start doing additional experiments. I plan to explore the size separation…

Posted in NRG

DNA translocations through ALD-coated NPN

First off, a quick update on the state of the lab. The day finally came, we had to pack up and put everything in storage, so unless there is a very pressing need, I’m done data collection for the time…

Posted in NRG

Size separation of DNA with NPN pre-filters

Since my last update I have been trying to achieve reliable size-separation of DNA by length using dwell time with the NPN pre-filter. Originally I had hoped to achieve 250-bp resolution near the optimal length for the NPN filter devices…

Posted in NRG

Update on progress with size separation and ALD

This update covers my efforts since our last skype meeting to show DNA size separation in a filter, as well as some very interesting TEM images of ALD-coated NPN and associated controls. Here is an inventory of my current chips:…

Posted in NRG

Control Experiments for NPN Translocation Project

Just a quick update this time – since my last post I have been doing control experiments to demonstrate the effect of the filters. For the controls I have been using the chips without the nitride cap, since I am…

Posted in NRG

Update on entropy tricks with NPN

Since my last update things have been going quite smoothly. Most pores I make are able to pass 3 or 4 samples before clogging, and I have filled in the various graphs quite nicely. I still would like to flesh…