concentration curve for PBS + Rhodamine

I mixed made solutions of PBS and Rhodamine with varying Rhodamine concentrations and ran them through the spectrometer. Below is the concentration vs absorption curve I made from it. I blanked the spec with PBS instead of ddH2O since the…

Posted in NRG

stir cell

Art is going to make a second stir cell this week. I asked him to replicate it as closely as possible, however I’m not sure how well that’s going to work. The one we currently have is made out of…

Posted in NRG

Human Albumin/Cytochrome C diffusion cell

I ran another diffusion cell last week using Human Albumin and Cytochrome C. I increased the volume of PBS because the last time I ran the gel for this mixture, the band for cytochrome c was very prominent. Out of…

Posted in NRG

Rhodamine Dilution Graph

I re-ran the rhodamine dilutions narrowing in on the molarities within the range readable by the spectrometer. My start sample was .5mM of Rhodamine. The wavelength I set the spectrometer at was 530nm with 3 trials of each dilution. I…

Posted in NRG

Updated Rhodamine Dilution

I fixed the graph for the serial dilution of Rhodamine that I did last week and removed all absorbency values that were greater than 1.08 AU. The graph looks much more linear now with an R^2 value of .9517

Posted in NRG

Serial Dilution of Rhodamine

I ran a series of serial dilutions with the rhodamine, to find the absorbency using the spectrometer. Below is a graph of the concentration of rhodamine versus the absorbency. I removed the concentrations which had absorbances greater than 1.7 AU…

Posted in NRG

Diffusion Cell: blood protein

Last week Jess helped me set up the diffusion cell with human albumin and cytochrome c. We ran 3 cells and used membranes from wafer 565. The membranes used were -1,4 (retentate 1), 3,3 (retentate 2), and 4,2 (retentate 3).…

Posted in NRG

Gel from Diffusion Chamber

Jess showed me how to use the diffusion chamber to separate proteins on the membranes. I ran a gel to see if any proteins appeared in the filtrate. The gel is posted below: The lanes are (from left): protein standard,…

Posted in NRG Tagged with:

Serial Dilution of Rhodamine

I was having trouble using the spectrometer to measure rhodamine concentration in the stir cell. I ran a standardized absorbency of the serial dilution of rhodamine. The curve is posted below. It appears to be linear. The molarity of rhodamine…

Posted in NRG Tagged with: ,

Rhodamine concentration curve

Lingyun and I used the stir cell and spectrometer to measure the diffusion of rhodamine across the membrane. This was the first time I was able to construct an experiment in the stir cell while keeping both membranes intact. In…

Posted in NRG Tagged with: ,
0
    0
    Your Cart
    Your cart is emptyReturn to Shop