Author: Rachel Twardowski

Diffusion Stir Cell w microbeads

Mike and I tried to pass 3 um beads mixed with rhodamine through the stir cell to prove that, if the membrane we intact, only the rhodamine would pass through and not the beads. As seen in the pictures below,…

Posted in NRG Tagged with: , ,

Diffusion Cell

I ran a few tests with rhodamine to see if the fluorescence will transfer across the cell. The problem I keep having is that the stir cell set-up is very sensitive. If the wing nuts are tightened too much the…

Posted in NRG Tagged with: ,