Category: NRG

HUVEC Adherence on Microporous Membranes Under Flow

Introduction/Motivation Endothelial cell adherence mechanisms are well characterized in literature to date. Endothelial cells, such as HUVECs, interact with their substrate as well as surrounding cells through focal adhesions (network of proteins involved in cell adhesion; vinculin, talin, FAK, etc.),…

Posted in NRG

Parylene microporous membranes

I am developing a process for fabricating microporous Parylene Liftoff membranes. I am interested in these as a more flexible substrate for cell culturing.  Parylene is relatively strong (compared to say pdms), so it is feasible to work with lifted…

Posted in NRG

Thin (5 nm) Au layer TEM imaging on 1148 NPN/npMgF2

Intro Understanding how the Au film coats the inner part of the npMgF2 is essential to understanding how the photonic properties of the npAu/npMgF2 sensor arise. From SEM, we are able to resolve little cones of Au, but unable to…

Posted in NRG

Tour de force analysis of NPN/NPN-O pores

Many thanks to JK, Dean and Gunner (Webster HS) for compiling this table. Take homes … NPN-O has smaller pore sizes, lower porosity than NPN at the same thickness (50 nm). All materials have slightly asymmetric pores (~ R1/R2 =…

Posted in NRG

Updated PETL Dialysis Images

Within the past few weeks we have been working on finalizing an architecture for PETL dialysis that can be cut out, assembled, and disassembled repetitively with precision. Within the past week we were able to replicate the results Kilean achieved…

Posted in NRG

Updated Post on How to Add LaTex to Your Posts

I know this is my third post today, but this is not a data post. It’s more of a PSA. If you want to add beautiful equations into your post (like I did here) then rather than generating a bunch…

Posted in NRG

Exosome Capture from Fresh Human Plasma

This data is from about a month ago and it something that Jim has been asking me to put up, so here it finally is. When Tejas runs his experiments, he usually leaves me the last mL of blood that…

Posted in NRG

Particle Capture on Pores

Last summer, Tejas and I spent a few days beating our heads against the wall because I was trying to develop a mathematical model of particle capture. Specifically, I was trying to understand what amount of transmembrane pressure we would…

Posted in NRG

Process Variables to imitate wafer 1085 npMgF2/npAu

Summary I want to imitate the material properties from 1085 as they have given us the best SERS performance to date. We have the best information that we’ve ever had before imitating the nanostructure and nanotopology from the MgF2. Our…

Posted in NRG

Update on Track Etched Membranes Experiments

Hello Everyone, As you probably remember, We have been working on optimizing Track Etched membranes devices since last semester, these membranes are 80 nm pore size and our beads are 100 nm in. We have been working on the design to…