Wafer #240802-02 – 8 Micron Microslit

Manufacturer’s Data Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  8 Micron MicroSlit SKU: MPSN400.C-3LX.1-8K32 Lot Number: 240802-02 Quantity Received: 220 Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 3.7 2psi: 5.66 4psi: 8.39 Burst:…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5250 – 8 Micron Microslit

Manufacturer’s Data Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  8 Micron Microslit SKU: MPSN400.C-3LX.1-8K32 Lot Number: 5250 Quantity Received: 320 Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 5.482 2psi: 8.66 4psi: 13.389 Burst:…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5252 – 8 Micron Microslit

Manufacturer’s Data Delivery Date: 8/20/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  8 Micron Microslit SKU: MPSN400.C-3LX.1-8K32 Lot Number: 5252 Quantity Received: 340 Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 5.077 2psi: 7.325 4psi: 10.608 Burst:…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5251 – 8 Micron Microslit

Manufacturer’s Data Delivery Date: 8/20/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  8 Micron Microslit SKU: MPSN400.C-3LX.1-8K32 Lot Number: 5251 Quantity Received: 340 Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 6.65 2psi: 9.52 4psi:  14.36 Burst:…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5209 – 8 Micron Microslit

Manufacturer’s Data Delivery Date: 7/11/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  8 Micron Microslit SKU: MPSN400.C-3LX.1-8K32 Lot Number: 5209 Quantity Received: 240 Manufacturer Test Report: Pore Size: Flow Data Avg in SLPM 2psi: 4psi: Burst: UR Testing…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5243- 0.5 μm Microporous

Manufacturer’s Data Delivery Date: 8/20/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  MPSN 0.5 Microporous SKU: MPSN400.C-3LX.1-0.5L1 Lot Number: 5243 Quantity Received: 150 Manufacturer Test Report: Pore Size: N/A Flow Data Avg in SLPM 2psi: 1.98 4psi: 4.393…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5244- 0.5 μm Microporous

Manufacturer’s Data Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  MPSN 0.5 Microporous SKU: MPSN400.C-3LX.1-0.5L1 Lot Number: 5244 Quantity Received: 250 Manufacturer Test Report: Pore Size: 530.14 nm Flow Data Avg in SLPM 2psi: 1.775 4psi:…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5246- 0.5 μm Microporous

Manufacturer’s Data Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  MPSN 0.5 Microporous SKU: MPSN400.C-3LX.1-0.5L1 Lot Number: 5246 Quantity Received: 200 Manufacturer Test Report: Pore Size: 536. 22 nm Flow Data Avg in SLPM 2psi: 1.273…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5245- 0.5 μm Microporous

Manufacturer’s Data Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  MPSN 0.5 Microporous SKU: MPSN400.C-3LX.1-0.5L1 Lot Number: 5245 Quantity Received: 250 Manufacturer Test Report: Pore Size: 525.12 Flow Data Avg in SLPM 2psi: 1.418 4psi: 3.155…

Posted in MPHH Blog, Wafer QC Pages

Wafer #5242- 0.5 μm Microporous

Manufacturer’s Data Delivery Date: 7/26/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  MPSN 0.5 Microporous SKU: MPSN400.C-3LX.1-0.5L1 Lot Number: 5242 Quantity Received: 210 Manufacturer Test Report: Pore Size: 478.08 nm Flow Data Avg in SLPM 2psi: 1.177 4psi:…

Posted in MPHH Blog, Wafer QC Pages