Category: Wafer QC Pages

Wafer #240701-05 – 1 Micron Microslit

Manufacturer’s Data Delivery Date: 8/25/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  1 Micron MicroSlit SKU: MSSN400.C-3LX.1-1.0E2 Lot Number: 240701-05 Quantity Received: 250 Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 1.83 2psi: 3.47 4psi: 6.34 15psi:…

Posted in MPHH Blog, Wafer QC Pages

Wafer #240919-13 – 2 Slot NPN

Manufacturer’s Data Delivery Date: 3/26/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 2 Slot Wide Short SKU: NPSN100.C-2LZ.4 Lot Number: 240919-13 Quantity Received: 70 Manufacturer Test Report: Pore Size: 63.2 nm Porosity: 22.9% Flow Data Avg in…

Posted in Wafer QC Pages

Wafer #240803-20 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 4/14/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240803-20 Quantity Received: 220 Manufacturer Test Report: Pore Size: 51 nm Porosity: 12% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #240919-16 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 6/3/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240919-16 Quantity Received: N/A Manufacturer Test Report: Pore Size: 60.3 nm Porosity: 17.1% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #240919-25 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 4/28/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240919-25 Quantity Received: 370 Manufacturer Test Report: Pore Size: 67.3 nm Porosity: 22.8% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #240919-18 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 4/29/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240919-18 Quantity Received: 320 Manufacturer Test Report: Pore Size: 61 nm Porosity: 18% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #240919-17 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 4/28/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240919-17 Quantity Received: 360 Manufacturer Test Report: Pore Size: 63.2 nm Porosity: 17.1% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #24240803-19 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 6/3/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 24240803-19 Quantity Received: N/A Manufacturer Test Report: Pore Size: 46.5 nm Porosity: 11.3% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #240919-14 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 6/4/2025 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240919-14 Quantity Received: N/A Manufacturer Test Report: Pore Size: 63.8 nm Porosity: 24.5% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages

Wafer #240803-15 – 1 Slot NPN

Manufacturer’s Data Delivery Date: 12/23/2024 (picked up and logged by Ahmet Gurcan) Membrane Type:  NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240803-15 Quantity Received: 340 Manufacturer Test Report: Pore Size: 57 nm Porosity: 17% Flow Data Avg in SLPM 2psi:…

Posted in Wafer QC Pages