HMM vs. LMM diffusion

My last post dealing with this project was the first to definitively demonstrate HMM diffusion through pnc-Si.  Unfortunately, there wasn’t a difference between the HMM filtrate signal for intact and digested (+RNAse) samples.  As a reminder, HMM is a large…