Tag: cell culture

Effect of salt on pores (benchtop)

(Transferred from old blog) The above TEM images show that RTP (800C, 5 min) treated samples (from W334) have their pores intact in salt over a period of time! 1M and 2M NaCl solutions were used and TEM samples were…

Posted in NRG Tagged with: , ,

pH Variation of DMEM

(Transferred from old blog) Aim: Determine how quickly DMEM pH changes once removed from the incubator Methods and Materials: • non-sterile complete Dulbecco’s Modified Eagle’s Medium (DMEM) supplemented with 10% FBS • 6 and 24 well cell culture plates •…

Posted in NRG Tagged with: ,

HUVEC Growth on Si

Over the past five days Anant and I monitored human umbilical vein endothelial cell (HUVEC) proliferation on three substrates: RTP-treated Si samples (both with and without membranes), glass (microscope coverslips), and plastic (6-well tissue culture plates). After the first two…

Posted in NRG Tagged with: , ,