Fibroblast Adhesion Update

Four more adhesion experiments were carried out and the results can be seen in the following charts. Based on the average of the four trials it can be elucidated that the initial adhesion (after ~7 hours) is pretty much the…

Posted in NRG Tagged with: , ,

Cell Adhesion Testing 6/3-6/4

Two more adhesion tests were run recently, one on Tuesday and one on Wednesday. For both tests cells were imaged after five hours. Fibroblast trial 3 was the first test where the optimal cell density (assuming 100% of cells are…

Posted in NRG Tagged with: , ,

HUVEC and Fibroblast Growth Summary

Thus far three HUVEC and two L13T3 growth tests have been conducted on substrates including glass,pnc-Si, tissue culture plastic, and untreated plastic. Only one test with untreated plastic has been run for each cell type. Cells on Si samples are…

Posted in NRG Tagged with: , ,

Adhesion Testing: HUVEC and Fibroblasts

Adhesions tests are being performed to see if cellular attachment varies between our material, glass, and plastic. These experiments are motivated by lower initial cell densities observed on pnc-Si in growth tests; we are investigating if the lower initial densities…

Posted in NRG Tagged with: , ,

HUVEC growth curve

HUVEC (P5) growth was monitored over 3 days on different substrates (glass coverslips, tissue culture treated & untreated plastic and RTPed pnc-Si from W510). The growth curve is as shown below and it can be observed that the growth rate…

Posted in NRG Tagged with: ,

Fibroblast Growth Take 3

A third fibroblast (L1 3T3, P22) growth test was conducted using glass, untreated and tissue culture treated plastic, and RTPed pnc-Si (W509) as substrates. Cells were grown in DMEM +10% FBS changed every 48 hours. R values are for the…

Posted in NRG Tagged with: ,

HUVEC Growth and associated pnc-Si discoloration

HUVEC (P8) growth was monitored over 5 days on different substrates (glass coverslips, tissue culture treated plastic and pnc-Si from W510). The growth curve is as shown below and it can be observed that the growth rate on pncSi in…

Posted in NRG Tagged with: ,

Fibroblast Growth and Associated pnc-Si Discoloration

A second fibroblast (L1 3T3, P21) growth test was conducted on RTP treated samples from W510, tissue culture plastic (polystyrene), and glass cover slips. Fibroblasts were cultured in DMEM with media changed every 48 hours. Cells were imaged using the…

Posted in NRG Tagged with: , , ,

HUVEC Growth on Si: Take 2 and 3

Last week I attempted another HUVEC growth study on Si, coverslips (glass), and culture wells (plastic). The cells were seeded at too low of a density on the membrane so I adjusted my protocol and started a third growth test.…

Posted in NRG Tagged with: , ,

Incubator versus Benchtop

(Transferred from old blog) From the above discoloration array it can be inferred that the RTP treated samples in the incubator are discoloring in much slower rate than the ones on the benchtop. Thus, incubator conditions prevent the chips from…

Posted in NRG Tagged with: , ,
0
    0
    Your Cart
    Your cart is emptyReturn to Shop