Electron Beam Evaporator Protocol

Electron Beam Evaporator Protocol (V_1.0) – Lingyun Here is the first version protocol of the electron beam evaporator at RIT clean room. There is not too much to put down here – the best way to learn this is to…

Posted in NRG Tagged with: , , ,

New metal coated wafer#502

Wafer#502 was coated with 10nm_Ti & 15nm_Au on Friday. I will pick out pinhole free membranes later today. I will also try to get TEM images at Karen’s lab (medical center). // The RIT clean room is closed this week.

Posted in NRG Tagged with: ,

Diffusion Cell New Designs

Here are two new designs for the new diffusion cells. Design_2 could be a better solution as it separates the two connections and uses screws to make the wire contacts to outside circuit. Please feed back any ideas to improve…

Posted in NRG Tagged with: , , ,