New metal coated wafer#502

Wafer#502 was coated with 10nm_Ti & 15nm_Au on Friday. I will pick out pinhole free membranes later today. I will also try to get TEM images at Karen’s lab (medical center). // The RIT clean room is closed this week.

Posted in NRG Tagged with: ,