Karl's Air Permeability and Burst Pressure Raw Data

In this week’s meeting there was a request to have Maryna and I make our BP and AP data available online. While Maryna is at the Gordon Conference I thought I would upload what I have. The attached spreadsheet contains…

Posted in NRG Tagged with: ,

W565 Air Permeability and Burst Pressure

I tested four samples (-1,1); (-1,2); (-1,3); and (-2,4) for air permeability and burst pressure. The first three samples showed no measurable air permeability for three attempts each. The sample from position (-2,4) did have a very small air permeability…

Posted in NRG Tagged with: ,

W502 and 504 Testing

W502 and 504 were tested for burst pressure and air permeability. Only one sample from W502 was tested for burst pressure (the other broke while setting up and I wanted to conserve samples) with a burst pressure of 4.46 psi.…

Posted in NRG Tagged with: ,