Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 2 Slot SKU: NPSN100.C-2LZ.4 Lot Number: 250410-15 Quantity Received: 110 Notes: Manufacturer Test Report: Pore Size: 45.5 nm Porosity: 21.8% Flow Data Avg in SLPM 1psi: 0.26 2psi: 0.51 Burst: 2.85…