Author: Ahmet Gurcan

Wafer #250410-11 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-11 Quantity Received: 380 Manufacturer Test Report: Pore Size: 34.9 nm Porosity: 11.3% Flow Data Avg in SLPM 1psi: 0.06 2psi: 0.12 Burst: 5.18 PSI…

Posted in Wafer QC Pages

Wafer #250410-08 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-08 Quantity Received: 310 Manufacturer Test Report: Pore Size: 50.4 nm Porosity: 22% Flow Data Avg in SLPM 1psi: 0.16 2psi: 0.33 Burst: 2.76 PSI…

Posted in Wafer QC Pages

Wafer #250410-01 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-01 Quantity Received: 340 Manufacturer Test Report: Pore Size: 43.5 nm Porosity: 14.9% Flow Data Avg in SLPM 1psi: 0.09 2psi: 0.17 Burst: 4.75 PSI…

Posted in Wafer QC Pages

Metal Contamination in Cryomilled Microplastic Reference Particles: Source, Dose, and Cytotoxicity Benchmarking

Cryomilling polymer feedstock into microplastic reference particles introduces metal from the milling hardware. We measured it by ICP-MS, traced it to its source, and benchmarked it against published cytotoxicity thresholds. This post reports what we found, including the parts that…

Posted in Microplastics

Wafer #240913-25 – 1 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 1 micron Microslit SKU: MSSN400.C-3LX.1-1.0E2 Lot Number: 240913-25 Quantity Received: 340 Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 1.67 2psi: 3.1 4psi: 5.19 15psi: 11.87 Burst: 39.9 PSI

Posted in NRG

Wafer #250409-06 – 1 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 1 micron Microslit SKU: MSSN400.C-3LX.1-1.0E2 Lot Number: 250409-06 Quantity Received: 160 Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 5.1 15psi: 11.87 Burst: 45.45 PSI

Posted in NRG

Wafer #240918-24 – 1 μm Microslit – Gold Coated

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 1 micron Microslit – Gold Coated SKU: MSSN400.C-3LX.1-1.0E2-AU Lot Number: 240918-24 Quantity Received: 200 Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 4.5 15psi: 10.58 Burst: 66.78 PSI

Posted in NRG

Wafer #251028-10 – 8 μm Microslit – Gold Coated

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 8 micron Microslit – Gold Coated SKU: MSSN400.C-3LX.1-8.0K2-AU Lot Number: 251028-10 Quantity Received: 200 Manufacturer Test Report: Flow Data Avg in SLPM 15psi: 7.6 Burst: 16.1 PSI

Posted in NRG

Wafer #250409-13 – 0.5 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 0.5 micron Microslit SKU: MSSN400.C-3LX.1-0.5E1 Lot Number: 250409-13 Quantity Received: 250 Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 3.96 15psi: 14.4 Burst: 9.82 PSI

Posted in NRG

Wafer #251028-02 – 0.5 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 0.5 micron Microslit SKU: MSSN400.C-3LX.1-0.5E1 Lot Number: 251028-02 Quantity Received: 250 Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 3.88 15psi: N/A Burst: 9.22 PSI

Posted in NRG