Author: Ahmet Gurcan

Wafer #250413-10 – 5 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 5 micron Dual Scale SKU: DSSN100.C-1LZ.0-5.0B2 (1.25% Porosity – Not real porosity) Lot Number: 250413-10 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 12.2% Average Diameter (microporous): 5 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #250413-17 – 5 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 5 micron Dual Scale SKU: DSSN100.C-1LZ.0-5.0B2 (1.25% Porosity – Not real porosity) Lot Number: 250413-17 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 12.16% Average Diameter (microporous): 5 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240914-16 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240914-16 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 9% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240917-15 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0.A. (0.63% Porosity – Not real porosity) Lot Number: 240917-15 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 15.4% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240917-13 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240917-13 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 14.4% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240917-12 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240917-12 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 11.3% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240919-11 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240919-11 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 22.4% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240919-10 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240919-10 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 21.6% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240922 – 1 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 1 micron Microslit SKU: MSSN400.C-3LX.1-1.0E2 Lot Number: 240922 Quantity Received: Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 1.67 2psi: 3.22 4psi: 5.77 15psi: 14.71 Burst: 39.59 PSI UR Testing…

Posted in Wafer QC Pages

Wafer #240919-24 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240919-24 Quantity Received: Manufacturer Test Report: Pore Size: 52.6 nm Porosity: 8.5% Flow Data Avg in SLPM 2psi: 0.107 4psi: 0.201 Burst: 3.63 PSI UR…

Posted in Wafer QC Pages