Author: Ahmet Gurcan

Wafer #240914-11 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-11 Quantity Received: Manufacturer Test Report: Pore Size: 52.2 nm Porosity: 16.4% Flow Data Avg in SLPM 1psi: 0.11 2psi: 0.19 Burst: 3.63 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-10 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-10 Quantity Received: Manufacturer Test Report: Pore Size: 50.4 nm Flow Data Avg in SLPM 1psi: 0.236 Burst: 14.648 PSI UR Testing Porosity: Pore size:…

Posted in Wafer QC Pages

Wafer #240917-09 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240917-09 Quantity Received: Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 0.13 2psi: 0.25 Burst: 1.34 PSI UR Testing Porosity: Pore size: Pore morphology:…

Posted in Wafer QC Pages

Wafer #240917-05 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240917-05 Quantity Received: Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 0.21 2psi: 0.31 UR Testing Porosity: Pore size: Pore morphology: EDS: Membranes removed…

Posted in Wafer QC Pages

Wafer #240914-06 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-06 Quantity Received: Manufacturer Test Report: Pore Size: 65.4 nm Porosity: 13.5% Flow Data Avg in SLPM 1psi: 0.039 Burst: 3.31 PSI UR Testing Porosity:…

Posted in Wafer QC Pages

Wafer #240917-02 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240917-02 Quantity Received: Manufacturer Test Report: Pore Size: 65.9 nm Porosity: 18.6% Flow Data Avg in SLPM 2psi: 0.115 4psi: 0.223 Burst: 7.446 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-03 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-03 Quantity Received: Manufacturer Test Report: Pore Size: 40.3 nm Porosity: 12.6% Flow Data Avg in SLPM 2psi: 0.078 4psi: 0.33 Burst: 4.191 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-25 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240914-25 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 7.7% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #240914-04 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 3 micron Dual Scale SKU: DSSN100.C-1LZ.0-3.0A.1 (0.63% Porosity – Not real porosity) Lot Number: 240914-04 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 9.6% Average Diameter (microporous): 3 μm Average Diameter…

Posted in Wafer QC Pages

Wafer #250413-09 – 5 μm Dual Scale – Low Porosity

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 5 micron Dual Scale SKU: DSSN100.C-1LZ.0-5.0B2 (1.25% Porosity – Not real porosity) Lot Number: 250413-09 Quantity Received: Manufacturer Test Report: Average Porosity (nanoporosity): 9.7% Average Diameter (microporous): 5 μm Average Diameter…

Posted in Wafer QC Pages