Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 5 micron Dual Scale SKU: DSSN100.C-1LZ.0-5.0B2 (1.25% Porosity – Not real porosity) Lot Number: 250410-17 Quantity Received: 260 Manufacturer Test Report: Average Porosity (nanoporosity): 12.81% Average Diameter (microporous): 5 μm Average…