Wafer #250410-11 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-11 Quantity Received: 380 Manufacturer Test Report: Pore Size: 34.9 nm Porosity: 11.3% Flow Data Avg in SLPM 1psi: 0.06 2psi: 0.12 Burst: 5.18 PSI…

Posted in Wafer QC Pages

Wafer #250410-08 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-08 Quantity Received: 310 Manufacturer Test Report: Pore Size: 50.4 nm Porosity: 22% Flow Data Avg in SLPM 1psi: 0.16 2psi: 0.33 Burst: 2.76 PSI…

Posted in Wafer QC Pages

Wafer #250410-01 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250410-01 Quantity Received: 340 Manufacturer Test Report: Pore Size: 43.5 nm Porosity: 14.9% Flow Data Avg in SLPM 1psi: 0.09 2psi: 0.17 Burst: 4.75 PSI…

Posted in Wafer QC Pages

Wafer #250413-11 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-11 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 43.2 nm Porosity: 10.3% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.13 Burst: 6.7…

Posted in Wafer QC Pages

Wafer #250413-12 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-12 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 44.9 nm Porosity: 9.8% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.12 Burst: 7.43…

Posted in Wafer QC Pages

Wafer #250413-14 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-14 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 48.4 nm Porosity: 10.8% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.12 Burst: 7.98…

Posted in Wafer QC Pages

Wafer #250413-13 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-13 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 44.8 nm Porosity: 9.8% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.12 Burst: 7.32…

Posted in Wafer QC Pages

Wafer #2510022-13 – Non Porous

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: Non Porous SKU: SN400.C-3X.1 Lot Number: 2510022-13 Quantity Received: 250 Notes: UR Testing For more information visit:

Posted in Wafer QC Pages

Wafer #240913-22 – Non Porous

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: Non Porous SKU: SN400.C-3X.1 Lot Number: 240913-22 Quantity Received: 250 Notes: UR Testing For more information visit:

Posted in Wafer QC Pages

Wafer #250409-09 – 2 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 2 micron Microslit SKU: MSSN400.C-3LX.1-2.0K2 Lot Number: 250409-09 Quantity Received: 330 Notes: extra 100 in air filter disks Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 3.97 2psi: 5.61 4psi:…

Posted in Wafer QC Pages
0
    0
    Your Cart
    Your cart is emptyReturn to Shop